Abstract
Based on the advantages of Ni or Cu incorporation to the mechanical and tribological properties of nitride coatings, the co-incorporation of Ni and Cu at different ratios was employed on CrBN coatings. Results showed that Ni (11.01 at%) and Cu (3.41 at%) co-incorporation increased hardness from 24.4 GPa to 26.4 GPa. As a consequence, coatings wear rate decreased from 6.4 × 10−7 mm3/Nm to 5.4 × 10−7 mm3/Nm. At the meantime, friction coefficient declined from 0.30 to 0.28 due to CuO lubricating layer. However, when Cu content was high (10.68 or 15.05 at.%), the hardness of Ni-Cu-CrBN coatings sharply declined, which weakened wear resistance and increased friction coefficient. It indicated that Ni (11.01 at%) and Cu (3.41 at%) was the proper co-incorporation combination.
| Original language | English |
|---|---|
| Article number | 204167 |
| Journal | Wear |
| Volume | 488-489 |
| Online published | 2 Nov 2021 |
| DOIs | |
| Publication status | Published - 15 Jan 2022 |
Research Keywords
- CrBN coating
- Hardness
- Incorporation
- Plastic deformation
- Tribology
Fingerprint
Dive into the research topics of 'The mechanical and tribological properties of CrBN-Ni-Cu-O coatings with different Ni and Cu contents'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver