Abstract
The SCC behavior of Fe‐8.7 Al‐29.7Mn‐1.04C alloy in a 20% sodium‐chloride solution (100°C) has been investigated by the slow strain rate method. The results showed that the alloy was susceptible to SCC only at the free corrosion potential and at the applied strain rate of 2.8 × 10−7/s. Application of the cathodic potential during the slow strain rate test resulted in the loss of ductility in the alloy which was attributed to the hydrogen induced cracking. Copyright © 1986 Verlag GmbH & Co. KGaA, Weinheim
| Original language | English |
|---|---|
| Pages (from-to) | 444-447 |
| Journal | Materials and Corrosion |
| Volume | 37 |
| Issue number | 8 |
| DOIs | |
| Publication status | Published - Aug 1986 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Stress corrosion cracking of the austenitic Fe‐Al‐Mn alloy in chloride environment'. Together they form a unique fingerprint.Cite this