Abstract
Electrochemical corrosion and stress corrosion cracking (SCC) behavior of X80 steel in the sulfurated marine environment at open circuit potential and −850 mVSCE are investigated. The results show that SCC is controlled by both anodic dissolution and hydrogen evolution, which is attributed to the HSO3− acceleration of the anodic and cathodic current density. Localized anodic dissolution leads to pits, which induce stress that promotes the initiation of stress corrosion cracks. Under a cathodic potential of −850 mVSCE, the effect of dissolution is limited, and SCC susceptibility increases because of the synergistic effect of the high HSO3−concentration and cathodic potential. © 2023 The Authors.
| Original language | English |
|---|---|
| Pages (from-to) | 3925-3936 |
| Number of pages | 12 |
| Journal | Journal of Materials Research and Technology |
| Volume | 24 |
| Online published | 10 Apr 2023 |
| DOIs | |
| Publication status | Published - May 2023 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Research Keywords
- Cathodic potential
- HSO3−
- Stress corrosion cracking
- X80 steel
Publisher's Copyright Statement
- This full text is made available under CC-BY-NC-ND 4.0. https://creativecommons.org/licenses/by-nc-nd/4.0/
Fingerprint
Dive into the research topics of 'Stress corrosion cracking behavior of X80 steel under the combined effects of sulfide and cathodic potential'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver