Stress-Corrosion Cracking at Ceramic-Metal Interfaces

Research output: Chapters, Conference Papers, Creative and Literary WorksRGC 32 - Refereed conference paper (with host publication)peer-review

Abstract

It is known that the fracture resistance of glass-copper interfaces depends strongly on the water content in ambient gaseous environments. In the present study, subcritical crack growth stimulated by water and other environmental species is investigated for such interfaces. Tests were conducted in various liquids, namely water, N-methylformamide, and n-butanol. All were found to accelerate fracture with the greatest effects from liquid water. Results are considered in the context of current models for stress-corrosion crack growth.
Original languageEnglish
Title of host publicationJoining and Adhesion of Advanced Inorganic Materials
EditorsA.H. Carim, D.S. Schwartz, R.S. Silberglitt, R.E. Loehman
PublisherMaterials Research Society
Pages109-116
ISBN (Print)155899212
DOIs
Publication statusPublished - Apr 1993
Externally publishedYes
Event1993 MRS Spring Meeting - San Francisco, United States
Duration: 12 Apr 199316 Apr 1993
https://www.mrs.org/spring1993

Publication series

NameMaterials Research Society Symposium Proceedings
Volume314
ISSN (Electronic)0272-9172

Conference

Conference1993 MRS Spring Meeting
PlaceUnited States
CitySan Francisco
Period12/04/9316/04/93
Internet address

Fingerprint

Dive into the research topics of 'Stress-Corrosion Cracking at Ceramic-Metal Interfaces'. Together they form a unique fingerprint.

Cite this