Abstract
The addition of Cr and Ti elements gives V-4Cr-4Ti a ductile-to-brittle transition temperature as low as −140 ºC, significantly lower than that of pure V. However, the effect of oxygen solute on the deformability of V-4Cr-4Ti remains largely unexplored. Here, it is demonstrated that V-4Cr-4Ti exhibits significantly faster oxygen absorption kinetics compared to pure V. Although alloying with Ti can trap some oxygen solute, the remaining oxygen solute in the matrix severely embrittles the alloy. Profuse dislocation multiplication through kink formation and frequent cross-slips endows V-4Cr-4Ti with excellent low-temperature deformability. In contrast, oxygen-charged V-4Cr-4Ti containing 0.57 wt.% O shows severe embrittlement even at temperatures exceeding 200 ºC. High concentrations of oxygen solute, combined with Ti and Cr alloying elements, hinder dislocation motion, promote strain localization, and generate numerous super-jogs (sessile structures) and dislocation loops, collectively leading to embrittlement. These findings provide insights into the microscopic oxygen embrittlement mechanisms in V-4Cr-4Ti. © Youke Publishing Co., Ltd 2025.
| Original language | English |
|---|---|
| Pages (from-to) | 659-665 |
| Number of pages | 7 |
| Journal | Tungsten |
| Volume | 7 |
| Issue number | 3 |
| Online published | 25 May 2025 |
| DOIs | |
| Publication status | Published - Sept 2025 |
| Externally published | Yes |
Funding
This study was financially supported by the Continuous Basic Scientific Research Project (No. BJ020261223286).
Research Keywords
- Dislocations
- Embrittlement
- Oxygen
- Super-jog
- V-4Cr-4Ti
Fingerprint
Dive into the research topics of 'Microscopic mechanism of oxygen embrittlement in V-4Cr-4Ti alloy'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver