Abstract
The pure and Sm modified SrTiO3 ceramics have been fabricated by solid state reaction method at different atmospheres, including ambient, reduced and oxidized conditions. All studied ceramics are in single cubic perovskite phase with high bulk density, where Sm doped ceramics possess decreased grain size. The room temperature permittivities of Sr0.97Sm0.02TiO3 and Sr0.98Sm0.02TiO3 sintered in N2 were found to be on the order of 25120 and 13370 at 1 kHz with dielectric loss being 0.044 and 0.008. The giant permittivities were associated with the increase of Ti3+ ions, which were due to the combination of Ti4+ ions and electrons. With increasing Ti3+ ions, the concentration of Ti4+ ions, Ti3+ ions and VO·· reach the balance where the defect dipoles [Ti4+·e-VO··-Ti4+·e] were created, responsible for the low dielectric loss. © 2018, Springer Science+Business Media, LLC, part of Springer Nature.
| Original language | English |
|---|---|
| Pages (from-to) | 11546-11552 |
| Journal | Journal of Materials Science: Materials in Electronics |
| Volume | 29 |
| Issue number | 13 |
| DOIs | |
| Publication status | Published - 1 Jul 2018 |
| Externally published | Yes |
Bibliographical note
Publication details (e.g. title, author(s), publication statuses and dates) are captured on an “AS IS” and “AS AVAILABLE” basis at the time of record harvesting from the data source. Suggestions for further amendments or supplementary information can be sent to [email protected].Funding
Acknowledgements This work was supported by NSFC-Guangdong Joint Funds of the Natural Science Foundation of China (No. U1601209), the National Key Basic Research Program of China (973 Program) (No. 2015CB654601) and Natural Science Foundation of China (No. 51372191).