LOCALIZED CORROSION BEHAVIOUR OF Ni-BASE SUPERALLOYS.

Research output: Journal Publications and Reviews (RGC: 21, 22, 62)22_Publication in policy or professional journal

3 Scopus Citations
View graph of relations

Author(s)

Detail(s)

Original languageEnglish
Pages (from-to)251-253
Journal / PublicationMetals Forum
Volume7
Issue number4
Publication statusPublished - Mar 1984
Externally publishedYes

Abstract

The representative nickel-based superalloys used for corrosion resisting purposes are Hastelloy C-276 and Inconel 625. Aspahani has reported that alloy 625 is subject to pitting and crevice corrosion in oxidized chloride environments whereas alloy C-276 performs well. However, according to Needham et al. , alloy C-276 suffers crevice corrosion in concentrated acid. The study investigated localized corrosion of C-276 and 625 in neutral and acidic chloride-containing environments at room and elevated temperatures.

Citation Format(s)

LOCALIZED CORROSION BEHAVIOUR OF Ni-BASE SUPERALLOYS. / Tjong, S. C.

In: Metals Forum, Vol. 7, No. 4, 03.1984, p. 251-253.

Research output: Journal Publications and Reviews (RGC: 21, 22, 62)22_Publication in policy or professional journal