High-cycle fatigue of nickel-base superalloy René 104 (ME3): Interaction of microstructurally small cracks with grain boundaries of known character

  • Yong Gao
  • , J.S. Stölken
  • , Mukul Kumar
  • , R.O. Ritchie*
  • *Corresponding author for this work

Research output: Journal Publications and ReviewsRGC 21 - Publication in refereed journalpeer-review