Heterogeneous structures in a Ni-based superalloy with tailoring mechanical properties produced by a twin laser powder bed fusion system

Research output: Journal Publications and Reviews (RGC: 21, 22, 62)21_Publication in refereed journalpeer-review

1 Scopus Citations
View graph of relations

Author(s)

  • Chuan Guo
  • Zhuoyu Li
  • Yuhe Huang
  • Minglin He
  • Qingqing Li
  • Yang Zhou
  • Fan Zhou
  • Gang Ruan
  • Wangqing Wu
  • Qiang Zhu

Related Research Unit(s)

Detail(s)

Original languageEnglish
Article number166983
Journal / PublicationJournal of Alloys and Compounds
Volume927
Online published27 Aug 2022
Publication statusPublished - 15 Dec 2022

Abstract

Powder bed fusion using a laser beam (PBF-LB) is a promising additive manufacturing (AM) technology, used to produce components with complex geometry and design freedom. The parts are built in a layer-by-layer fashion during PBF-LB, and changing the processing parameters within different layers can lead to the modification of microstructures and finally a great impact on the mechanical properties. Thus, PBF-LB provides the possibility for the customization of material properties by changing the microstructures of layers using different processing parameters. In this investigation, a twin PBF-LB system, i.e., with a low-power laser beam and a high-power laser beam in a machine, is used to produce fine and coarse microstructures using the Inconel 718 (IN718) alloy, respectively. The fine and coarse microstructures are alternately printed to form different heterogeneous structures. Correspondingly, different mechanical properties are achieved. The microstructures are analyzed using optical microscope (OM), scanning electron microscope (SEM), electron backscatter diffraction (EBSD) and numerical calculation. The defects generated by these 2 laser beams are simultaneously discussed. This study facilitates the tailoring of alloy properties using the PBF-LB technology to meet the users’ needs of multiple service conditions.

Research Area(s)

  • Heterogeneous structure, Mechanical property, Microstructure, Nickel-based superalloy, Powder bed fusion

Citation Format(s)

Heterogeneous structures in a Ni-based superalloy with tailoring mechanical properties produced by a twin laser powder bed fusion system. / Guo, Chuan; Li, Zhuoyu; Huang, Yuhe et al.

In: Journal of Alloys and Compounds, Vol. 927, 166983, 15.12.2022.

Research output: Journal Publications and Reviews (RGC: 21, 22, 62)21_Publication in refereed journalpeer-review